Information is presented on the failure behavior of columnar-grained ice during compressive creep and constant strain rate tests. The role of crack formation in establishing the failure condition is briefly described. Breakdown of structure is responsible for a marked change in the creep behavior of ice in the stress range of 10 to 12 kg/cm2. A ductile-to-brittle transition is observed at a strain rate of about 5 × 10−3 min−1. The upper yield stress in constant strain rate tests is shown to increase with increase in rate of strain up to the ductile-to-brittle transition.


On présente des données sur le mécanisme de rupture de la glace à structure columnaire au cours d'essais de compression à charge constante (fluage) et à vitesse de déformation constante. L'importance de la formation des fissures pour établir les conditions de rupture est brièvement décrite. La fissuration de la structure est responsable des changements dans la progression du fluage de la glace pour des contraintes variant entre 10 et 12 kg/cm2. Une transition de l'état ductile à l'état fragile a été observée à un taux déformation d'environ 5 × 10−3 min−1. La limite apparente d'élasticité durant les essais à taux constant de déformation unitaire paraît augmenter avec une majoration du taux de déformation jusqu'au point de transition de l'état ductile à l'état fragile.